ASTM D5895 - Drying Time Recorder Equipment

CREEP TESTER TYPE

 

CREEP TESTER TYPE

PT. Mora Anugerah Berkat (M.A.B) adalah perusahaan yang bergerak di bidang alat laboratorium dan testing material, kami sudah mensupply berbagai alat keseluruh indonesia,khusus untuk material testing kami ingin menawarkan produk dari YASUDA SEIKI yang merupakan salah satu brand Jepang yang banyak di gunakan untuk pengujian material seperti : CREEP TESTER TYPE .

CREEP TESTER TYPE 

  • No.145-A/No.145-B CREEP TESTER (PULLEY TYPE/ BALANCE TYPE)

  • Standard Method : JIS-K7115, ASTM-D2990, ISO-899-1

  • This tester is used to measure the increasing creep by applying static load to plastic test specimens.

  • By choosing the Chuck, the tester enables to conduct tensile test, condensation test, and bending test.

  • The tester can also be assorted with test functions such as relaxation test, heat shrinkage test, and thermal impulse test.

  • Click Here : CREEP TESTER (PULLEY TYPE/BALANCE TYPE)


CREEP TESTER (PULLEY TYPE/ BALANCE TYPE)
ModelCREEP TESTER (PULLEY TYPE)
Hangings3, 6, or 10 Hangings (3 kinds)
SpecimenSee JIS-K7162 for reference JIS-K7162
Load MethodPulley Wheel Type
Weight LoadMax. 500 N (50 kgf)
Displacement
Measurement
Potentiometer :
Scale 0.1 mm, Stroke 0 to Max. 300 mm
Differential Transformer :
Scale 0.01 mm, Stroke 0 to Max. ± 40 mm
Temperature
Range
Max. 200 °C
SoftwareWindows Compatible
OptionCompression Jig, Bending Jig, Low Temperature Oven,
Constant Temperature & Humidity Oven, Divided Oven,
Liquid Immersion Bath, Gauge Length Measuring Spec,
Weight Traveling System (WTS)
Power SourceDiffer by Specifications.
Dimensions /
Weight (Approx.)
Differ by Specifications.
CREEP TESTER (PULLEY TYPE/ BALANCE TYPE)
ModelCREEP TESTER (BALANCE TYPE)
Hangings3, 6, or 10 Hangings (3 kinds)
SpecimenSee JIS-K7162 for reference JIS-K7162
Load MethodBalance Scale Type
Weight LoadMax. 5 kN (500 kgf)
Displacement
Measurement
Differential Transformer :
Scale 0.01 mm, Stroke 0 to Max. ± 40 mm
Temperature
Range
Max. 200 °C
SoftwareWindows Compatible
OptionCompression Jig, Bending Jig, Low Temperature Oven,Constant Temperature & Humidity Oven, Divided Oven,Liquid Immersion Bath, Gauge Length Measuring Spec,Weight Traveling System (WTS)
Power SourceDiffer by Specifications.
Dimensions /
Weight (Approx.)
Differ by Specifications.

==========================

  • No.145-SV CREEP TESTER (SERVOMOTOR TYPE)

  • Standard Method : JIS-K7115, ASTM-D2990, ISO-899-1(CREEP TEST), JIS-K6263, ISO-3384(STRESS RELAXATION TEST)

  • Adding a servomotor to the usual actual load type creep tester, and detecting the load using a load cell, the servomotor type creep tester can effectively reduce impact when the test specimen breaks, simultaneously saving space.

  • By choosing the Chuck, the tester enables conducting tensile stress relaxation tests and the condensation stress relaxation test.

  • The tester can also be assorted with test functions such as thermal contraction testing and thermal impact testing.

  • CLICK HERE : CREEP TESTER (SERVOMOTOR TYPE)



CREEP TESTER (SERVOMOTOR TYPE)
Specification
Hangings3, 6, or 10 Hangings (3 kinds)
SpecimenSee JIS-K7162 or JIS-K6263 for reference
Load MethodServomotor Type
Weight LoadMax. 5 kN (500 kgf)
Load DetectionLoad Cell
Displacement
Measurement
Potentionmeter :
Scale 0.1 mm, Stroke 0 to Max. 300 mm
Differential Transformer :
0.01 mm, Stroke 0 to Max. ± 40 mm
Temperature
Range
Max. 200 °C
SoftwareWindows Compatible
OptionCompression Jig, Bending Jig, Low Temperature Oven, Constant Temperature & Humidity Oven, Divided Oven, Liquid Immersion Bath, Gauge Length Measuring Spec
Power SourceDiffer by Specifications.
Dimensions /
Weight (Approx.)
Differ by Specifications.

==========================

  • HYBRID CREEP TESTER (STRESS RELAXATION TESTER)

  • Standard Method : JIS-K7115, ASTM-D2990, ISO-899-1(CREEP TEST), JIS-K6263, ISO-3384(STRESS RELAXATION TEST)

  • By equipping a load cell to the usual CREEP TESTER, this tester enables to test stress relaxation of vulcanized rubber and thermoplastic rubber.

  • By choosing the Chuck, the tester enables to conduct the tensile stress relaxation test and the condensation stress relaxation test.

  • The tester can also be assorted with test functions such as heat shrinkage test and thermal impulse test.

  • Click Here : HYBRID CREEP TESTER (STRESS RELAXATION TESTER)



HYBRID CREEP TESTER (STRESS RELAXATION TESTER)
Specification
Hangings3, 6 or 10 Hangings, (3 kinds)
SpecimenSee JIS-K6263 for reference
Load MethodPulley Wheel Type or Balance Scale Type
Load MeasuringLoad Cell, Max. 500 N (50 kgf)
Displacement
Measurement
Potentionmeter :
Scale 0.1 mm, Stroke 0 to Max.
Differential Transformer :
Scale 0.01 mm, Stroke 0 to Max. ± 40 mm
Temperature
Range
Max. 200 °C
SoftwareWindows Compatible
OptionCompression Jig, Bending Jig, Low Temperature Oven,
Constant Temperature & Humidity Oven, Divided Oven,
Liquid Immersion Bath, Gauge Length Measuring Spec
Power SourceDiffer by Specifications.
Dimensions / Weight 
(Approx.)
Differ by Specifications.

Jika anda membutuhkan/mencari alat CREEP TESTER TYPE . yang banyak di gunakan untuk pengujian material plastik,jangan ragu untuk menghubungi kami,marketing dan sales kami siap memjawab segala kebutuhan anda khususnya untuk alat uji Creep Test.

CREEP TESTER TYPE

Untuk informasi,pertanyaan dan pemesanan silahkan hubungi kami di :

  • PT. Mora Anugerah Berkat (M.A.B)

  • Alamat : Jl.Taman Asri Blok M No.36 Kel.Cipadu Kec.Larangan,Kota Tangerang - Provinsi Banten

  • Phone : 021 7345.7064

  • Mobile : 0812.8140.0749 / 0812.8770.5470 

  • Chat : Whats App, Line, WeChat, Telegram

  • Website : www.moraanugerah.id  -  www.moraanugerah.com

  • Email : info@moraanugerah.com - info@moraanugerah.id - marketing_div@moraanugerah.com